Common Trade Names: Hastelloy X, UNS N06002、GH3536、W.Nr.2.4665

Hastelloy X is a kind of nickel base superalloy with high iron content, which is mainly strengthened by solid solution of chromium and molybdenum. It has good anti-metallization and corrosion performance, medium endurance and creep strength below 900℃, good cold and hot processing formability and welding performance.
Used in the manufacture of aero-engine combustion chamber parts and other high temperature parts, under 900℃ for a long time, short time working temperature up to 1080℃.

Hastelloy X Chemical Composition

Alloy C Cr Ni Fe Mo W Al B Co Si Mn P S
Hastelloy X 0.05~0.15 20.5~23.5 balance 17.0~20.0 8.0~10.0 0.2~1.0 ≤0.1 ≤0.005 0.5~2.5 ≤1.0 ≤1.0 ≤0.015 ≤0.01

Hastelloy X Physical Properties

Density 8.3 g/cm³
Melting point 1260-1355 ℃

Hastelloy X Mechanical Properties

Status Tensile strength 
Rm N/mm²
Yield strength 
Rp 0. 2N/mm²
Elongation 
As %
Brinell hardness
HB
Solution treatment 690 275 30 >241

 

Hastelloy X  Standards and Specifications

Bar/Rod Wire  Strip/Coil Sheet/Plate Pipe/Tube Forging
 ASTM B572ASME SB572AMS 5754 AMS 5798 ASTM B435ASME SB435AMS 5536 ASTM B662,ASME SB662
ASTM B619,ASME SB619
ASTM B626 ,ASME SB626AMS 5587
AMS 5754

Hastelloy X Available Products in Sekonic Metals

Inconel 718 bar,inconel 625 bar

Hastelloy X Bars & Rods

Round bars/Flat bars/Hex bars,     Size From 8.0mm-320mm, Used for bolts,fastners and other spare parts

welding wire and spring wire

Hastelloy X Wire

Supply in welding wire and spring wire in coil form and cut length.

Sheet & Plate

Hastelloy X sheet & plate

Widths up to 1500mm and lengths up to 6000mm,Thickness from 0.1mm  to 100mm.

Hastelloy X seamless tube & Welded pipe

Standards size and  customized dimension can be produced by us with small tolerance

inconel strip,invar stirp,kovar stirp

Hastelloy X strip & coil

Soft condition and hard condition with AB bright surface, width up to 1000mm

Fasterner & Other Fitting

Hastelloy X Fasteners

Hastelloy X materials  in forms of Bolts,screws,flanges and other fasterners, according to clients specification.

Why Hastelloy X?

1. Excellent oxidation resistance at high temperature(>1200℃)).
2. Good high-temperature strength.
3. Good formability and weldability.
4. Good resistance to stress corrosion cracking.

Hastelloy X Application field:

Because of its corrosion resistance in various atmospheres at high temperature and excellent high temperature strength, HastelLoyx has been widely used in various high temperature environments.
Typical application fields:
• Industrial and aviation steam turbines (combustion chambers, rectifiers, structural caps)
• Industrial furnace components, support rollers, grates, ribbons and radiator tubes
• Spiral tubes in petrochemical furnaces
• High temperature gas cools the nuclear reactor

            

Sekonic metal Technology Co., Ltd. supply plate, strip, round steel, pipe, wire, forgings, ingot, flange, tee, elbow, complete specifications and models
material
Standard: Alloy steel F5 and 410;Stainless steel 304, 304L, 316, 316L, 321 and 347.
Non-standard: high nickel alloy (inconel 718, inconel 625, inconel 825, inconel 925, alloy 20,GH3030, nimoni 80A), high temperature alloy steel (haines 25,25, haines 188, etc.) and other stainless steel grades
Quality assurance, affordable price, short delivery time, provide the original factory warranty, if you need to welcome to call for consultation procurement mobile phone/whatsapp: 0086-15921454807